PPS - 40% GLASS FIBER
Reinforced glass fiber materials tend to crack due to their low tensile elongation, which means the larger scale the product
has, the higher cracking risk it gets. Therefore, we highly suggest being careful during cutting. Please heat the material to
80°C by a hot air circulating airbox before machining, or soak it in hot water remained 80°C for 3 to 4 hours. It is significant
to use a fine cutting tool during cutting and drilling. If it is for an ultra-precise part, please process it into a rough sample,
then anneal it again before finishing it.